3M EC-2216

Main features

  • Flexible Vibration Resistant Bonding
  • High Peel Structural Performance
  • Selectable Formulation Processing Window

Product Description

3M Scotch-Weld Epoxy Adhesive EC-2216 B/A is a flexible, room-temperature-curing epoxy for prepared metals, wood, plastics, rubber, and masonry exposed to shock, vibration, flexing, or thermal cycling. The gray formulation mixes 2:3 by volume, provides 90 minutes of work life, and reaches handling strength in 8 to 12 hours. The translucent formulation mixes 1:1 by volume, provides 120 minutes of work life, and reaches handling strength in 12 to 16 hours. Both formulations deliver 25 piw T-peel strength at 24 deg C.

Key features

  • Flexible Shock Resistant Bonding: The cured epoxy accommodates vibration, flexing, and thermal movement.
  • High Peel Structural Performance: Prepared joints combine peel and shear capability for demanding assemblies.
  • Gray Or Translucent Formulations: Distinct formulations support different mixing, handling, and appearance needs.

Applications

Flexible structural bonding of compatible metals, wood, plastics, rubber, masonry, and thermally cycled assemblies.

Product Family

3M EC-2216

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component SystemComponent System
Two (Accelerator | Base)
Other Properties
Storage TemperatureStorage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Gray and translucent formulations are separated because their mix ratios and processing windows differ.

PropertyValueUnitMethod / condition
Available formulationsGray; translucent-Select before processing
Gray mix ratio by volume2:3B:ATwo-part system
Translucent mix ratio by volume1:1B:ATwo-part system
Gray work life90min100 g mixed at 24 deg C
Translucent work life120min100 g mixed at 24 deg C
Technical properties

After-processing / final-state properties

Cured values remain separated by formulation where performance differs.

PropertyValueUnitMethod / condition
Gray hardness50 to 65Shore DASTM D2240
Translucent hardness35 to 50Shore DASTM D2240
Gray time to handling strength8 to 12hAt room temperature
Translucent time to handling strength12 to 16hAt room temperature
T-peel strength25piwBoth formulations; ASTM D1876 at 24 deg C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers