3M 784F
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Main features
- Fast Medium-Pressure Metal Grinding
- Flexible Wet-or-Dry Belt Grinding
- Grinding Aid for Heat-Sensitive Alloys
Product Description
3M Cubitron II Cloth Belt 784F is a polyester-backed abrasive belt that combines 3M Precision-Shaped Grain with premium aluminum oxide for medium-pressure metal grinding and blending. Grades 36+ to 80+ use a heavier YF-weight polyester backing, while grades 120+ to 180+ use a lighter XF-weight backing; both constructions are moderately flexible for flat and slight-contour work. The water-resistant backing allows wet or dry grinding, and an integrated grinding aid is included to reduce grinding temperatures on heat-sensitive alloys. The resin-bonded belt is designed for consistent cutting in industrial grinding and finishing operations while limiting changeouts in pressure-assisted and robotic use.
Key features
- Precision-shaped grain blend: The ceramic and aluminum oxide abrasive blend maintains a fast, consistent cut in medium-pressure grinding and blending.
- Flexible polyester backing: YF- and XF-weight polyester constructions provide moderate flexibility for flat surfaces and slight contours across the available grade range.
- Wet or dry grinding: The water-resistant backing allows wet or dry metalworking, while the grinding aid reduces heat generation on heat-sensitive alloys.
Applications
Use 3M Cubitron II Cloth Belt 784F for flat finishing, backstand grinding, cylindrical and centerless grinding, small bench grinders, inline sanders, and file-belt operations on metal.
TDS, SDS & Technical Documents
Technical Specifications
Other Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Abrasive mineral | 3M Precision-Shaped Grain and premium aluminum oxide blend | Product construction | |
| Grades available | 36+, 50+, 60+, 80+, 120+, 150+, 180+ | Product range | |
| Backing | YF-weight polyester | Grades 36+ to 80+ | |
| Backing | XF-weight polyester | Grades 120+ to 180+ | |
| Bond | Resin bond | Product construction | |
| Recommended storage temperature | 60 to 80 | deg F | Relative humidity 35 to 50% |